Öfeature |
Test Method |
2 V |
|
NLGI class |
- |
2 |
|
Drip point, °C |
ASTM D 556,D 2265 |
>260 |
|
Base oil viscosity@ 40 °C |
ASTM D 445 |
220 |
|
Penetration@ 25oC, mm-1 (60 hours) |
ASTM D217 |
265-295 |
|
Copper Corrosion Cu, max |
ASTM D 4048 |
1b |
|
Oil separation,% |
ASTM D1742 |
Max.5 |
|
Washing with water@80 °C, % |
ASTM D1264 |
Max 10 |
|
TIMKEN OK load test (IBS) |
ASTM D 2509 |
50 |
|
4 ball-wear test,mm |
ASTM D 2266 |
<0.6 |
|
4 ball-welding point test, kg |
ASTM D 2596 |
>280 |
|
Corrosion test |
ASTM D 1742 |
Pass |
| BARREL |